Spesifikasi
| Ciri | XS-FR-8800 | XS-FR-8801 | XS-FR-8802 | XS-FR-8802LC |
| Putihnya | ≥88 | ≥88 | ≥88 | ≥88 |
| Konten bromen % | 26 ± 3 | 6 ± 3 | 0.1 | 20 ± 3 |
| H ₂ O Konten % | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 |
| Kepadatan relatif | 1.5 ~ 1.7 | 1.1 ~ 1.2 | 1.5 ~ 1.7 | 1.5 ~ 1.7 |
| Kepadatan curah | ~ 0,8 | ~ 0,6 | ~ 0,8 | ~ 0,6 |
| Resistensi suhu | ★★★ | ★★★★ | ★★★★★ | ★★★★★ |
| Tahan curah hujan | ★★★ | ★★★★★ | ★★★★ | ★★★★ |
| Mobilitas | ★★★ | ★★★ | ★★★★★ | ★★★ |
| Suhu ekstrusi | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ |
| Binar kabel | GWIT 750 ℃ & GWFI 850 ℃ | |||
| Penerapan | Non fil | Isi/diperkuat | Temp. Resistensi Halogen rendah | Temp. Resistensi |
| Dosis % | XS-FR-8800 | XS-FR-8801 | XS-FR-8802 | XS-FR-8802LC | |||||||||
| Padding % | 0 | 15 | 30 | 0 | 15 | 30 | 0 | 15 | 30 | 0 | 15 | 30 | |
| Co-pp | 0.8mm V-2 | 2.5 | ———————————————————————————————————————————————————————— | —— | 2.5 | —— | —— | 2.5 | —— | —— | 2.5 | —— | —— |
| 1.6mm V-2 | 3 | —— | —— | 3 | —— | —— | 3 | —— | —— | 3 | —— | —— | |
| 3.2mm V-2 | 3 | —— | —— | 3 | —— | —— | 3 | —— | —— | 3 | —— | —— | |
| 0.8mm V-2 | 1 | —— | —— | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | |
| Ho-pp | 1.6mm V-2 | 1 | —— | —— | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 |
| 3.2mm V-2 | 1 | —— | —— | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | 1 | 2-3 | 4-5 | |
| Komentar | Beberapa pengisi akan mempengaruhi keterbelakangan api (seperti kalsium karbonat, magnesium karbonat, dll.) | ||||||||||||
| Ciri | XS-FR-8803 | XS-FR-8805 | XS-FR-8810 | XS-FR-8820 |
| Putihnya | ≥92 | ≥88 | ≥88 | ≥88 |
| Konten bromen% | 10 ± 3 | ≤2 | 0.1 | 20 ± 3 |
| H ₂ O Konten % | ≤0.5 | ≤0.5 | ≤1.0 | ≤1.0 |
| Kepadatan relatif | 1.6 ~ 1.8 | 1.1 ~ 1.2 | 1.5 ~ 1.7 | 1.5 ~ 1.7 |
| Kepadatan curah | ~ 0,8 | ~ 0,5 | ~ 0,8 | ~ 0,6 |
| Resistensi suhu | ★★★ | ★★★ | ★★★★★ | ★★★★★ |
| Tahan curah hujan | ★★★ | ★★★ | ★★★★ | ★★★★ |
| Mobilitas | ★★★ | ★★★ | ★★★★★ | ★★★ |
| Suhu ekstrusi | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ | ≤190 ℃ |
| Kawat cahaya | GWFI 800 ℃ | GWIT750 ℃/GWFI850 ℃ | ||
| Yang lain | Isi Kecil | Isi Kecil | Temp. Resistensi Halogen rendah | Temp. Resistensi |
| Dosis % | XS-FR-8803 | XS-FR-8805 | XS-FR-8810 | XS-FR-8820 | |||||||||
| Padding % | 0 | 5 | 30 | 0 | 5 | 30 | 0 | 15 | 30 | 0 | 15 | 30 | |
| Co-pp | 0.8mm V-2 | 2.5 | 3 | —— | 2.5 | 3 | —— | 3 | 3 | —— | 3 | 10 | —— |
| 1.6mm V-2 | 3 | 3.5 | —— | 3 | 3.5 | —— | 3.5 | 3.5 | —— | 3.5 | 10 | —— | |
| 3.2mm V-2 | 3 | 3.5 | —— | 3 | 3.5 | —— | 3.5 | 3.5 | —— | 3.5 | 10 | —— | |
| 0.8mm V-Z | 0.8 | 1 | —— | 0.8 | 1 | —— | 1 | 1 | —— | 1 | 6 | —— | |
| Ho-pp | 1.6mm V-2 | 0.9 | 1.2 | —— | 0.9 | 1.2 | —— | 1 | 1.2 | —— | 1 | 6 | —— |
| 3.2mm V-2 | 1 | 1.3 | —— | 1 | 1.3 | —— | 1 | 1.3 | —— | 1 | 6 | —— | |
| Komentar | Beberapa pengisi akan mempengaruhi keterbelakangan api (seperti kalsium karbonat, magnesium karbonat, dll.) Direkomendasikan untuk menambahkan barium sulfat, bubuk mika, manik -manik kaca, dll. Bedak harus tinggi konten silikon. Kombinasi sekrup geser yang kuat tidak disarankan untuk sekrup pencukuran; Tidak ada vakum atau vakum rendah dalam proses ekstrusi. | ||||||||||||
Fasilitas manufaktur di xusen
Dengan dua basis produksi yang berlokasi di Jiashan, Zhejiang, dan Juancheng, Shandong, kami saat ini mencapai kapasitas produksi tahunan 12.000 ton, yang terus berkembang. Kami bangga dengan laboratorium penelitian ilmiah tingkat provinsi Zhejiang kami. Kami memiliki lokakarya dan gudang produksi kami sendiri, dilengkapi dengan produksi lengkap dan peralatan inspeksi kualitas.
Mengapa Poliamida Standar Terbakar — dan Apa yang Dipecahkan oleh Format Masterbatch Poliamida – dikenal luas sebagai nilon – adalah salah satu plastik rekayasa paling populer di pasaran. PA6 da...
BACA SELENGKAPNYAAmonium polifosfat (APP) adalah salah satu penghambat api bebas halogen yang paling banyak digunakan di dunia, dan untuk alasan yang baik. Ini menggabungkan kandungan fosfor dan nitrogen yang tingg...
BACA SELENGKAPNYABahan penghambat api telah menjadi bagian standar dalam pembuatan polimer dan kabel selama beberapa dekade. Selama sebagian besar sejarah tersebut, bahan kimia yang dominan bergantung pada halogen—...
BACA SELENGKAPNYAMelamin Sianurat (MCA) adalah penghambat api bebas halogen yang dibentuk oleh kombinasi ekuimolar melamin dan asam sianurat. Hasilnya adalah bubuk putih kristal stabil yang telah menjadi sala...
BACA SELENGKAPNYA